摘要
利用腐蚀电化学以及浸泡腐蚀实验结果表明,通过向FLiNaK熔盐体系引入Cr2+/Cr3+氧化还原缓冲离子对,可以使不同金属材料在该熔盐体系的电位差缩小乃至消除,并抑制不同金属材料之间的电偶腐蚀。
关键词: 熔盐 ; 电偶腐蚀 ; 氧化还原缓冲离子对 ; 腐蚀抑制
Abstract
Galvanic corrosion should be considered when dissimilar metallic materials in contact with each other in a molten salt system of high ionic conductivity. Corrosion electrochemistry and immersion corrosion tests indicated that the difference of the corrosion potentials of different metal materials can be decreased or diminished by coupling Cr2+/Cr3+ into the 46.5%LiF-11.5%NaF-42.0%KF (in mole fraction) molten salt. Thus, the galvanic corrosion behavior between different metal materials can be effectively inhibited.
Keywords: molten salt ; galvanic corrosion ; redox buffering ion pair ; corrosion mitigation
![1.jpg](/d/file/dhTJDAOHANG/fhjs/jishuyingyong/2021-05-19/8a105a64309dd9ce3d01af1b513e143f.jpg)
免责声明:本网站所转载的文字、图片与视频资料版权归原创作者所有,如果涉及侵权,请第一时间联系本网删除。
相关文章
![](/skin/201904/index/img/ssdf.png)
官方微信
《中国腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62316606-806
- 邮箱:fsfhzy666@163.com
- 中国腐蚀与防护网官方QQ群:140808414
点击排行
PPT新闻
“海洋金属”——钛合金在舰船的
点击数:7130
腐蚀与“海上丝绸之路”
点击数:5741