摘要
综述了非晶合金耐蚀性的研究现状,归纳了合金成分、合金结构、制备工艺、腐蚀介质、表面状态、加载应力以及其他重要因素对非晶合金耐蚀性的影响规律,总结了非晶合金耐蚀性能的改善途径,并对非晶合金耐蚀性研究方面存在的问题和今后的发展趋势进行了探讨和展望。
关键词: 非晶合金 ; 耐蚀性 ; 影响因素 ; 改善方法
Abstract
Because of their unique amorphous structure, metallic glasses (MGs) exhibit better corrosion resistance compared with traditional crystalline metals and alloys. Thus, MGs have broad application prospects as novel corrosion-resistant materials. The research progress of corrosion resistance of MGs was summarized. The influence factors, such as the alloy composition, microstructure, preparation method, corrosion environment, surface state, stress state etc. on the corrosion resistance of MGs were introduced. The routes to improve the corrosion resistance of MGs were proposed. Finally, the future development trends of corrosion resistance of MGs were discussed and prospected.
Keywords: metallic glass ; corrosion resistance ; influence factor ; improving method
免责声明:本网站所转载的文字、图片与视频资料版权归原创作者所有,如果涉及侵权,请第一时间联系本网删除。
相关文章
官方微信
《中国腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62316606-806
- 邮箱:fsfhzy666@163.com
- 中国腐蚀与防护网官方QQ群:140808414
点击排行
PPT新闻
“海洋金属”——钛合金在舰船的
点击数:7130
腐蚀与“海上丝绸之路”
点击数:5741