1 | 加速腐蚀试验 accelerated corriosion test |
2 | 加速氧化 accelerated oxidation |
3 | 酸洗 acid cleaning |
4 | 酸洗清洁剂 acid picking |
5 | 酸洗清洁剂 acidic cleaner |
6 | 酸度 acidity |
7 | 活化 activity |
8 | 激化能 activation energy |
9 | 活化极化 activation polarization |
10 | 活化剂 activator |
11 | 活性的,活化的 active |
12 | 活化金属 active metals |
13 | 活化-钝化电池 active-passive cell |
14 | 活性区,活化区 active zone |
15 | 活度 activity |
16 | 优级海军黄铜 admiralty brass |
17 | 充气 aeration |
18 | 充气电池 aeration cell |
19 | 嗜氧菌 aerobic bacteria |
20 | 老化 aging |
21 | 老化作用 aging action |
22 | 大气污染 air pollution |
23 | 周浸试验 alternate immersion test |
24 | 厌氧菌 anaerobic bacteria |
25 | 厌氧菌腐蚀 anaerobic corrosion |
26 | 阴离子 anion |
27 | 阳极 anode |
28 | 阳极极化 anodic polarization |
29 | 阳极电流密度 anodic current density |
30 | 阳极氧化物膜 anodic oxide coating |
31 | 阳极保护 anodic protection |
32 | 阳极区电解质 anolyte |
33 | 耐侯性低合金钢 anti-weathering low alloy steel |
34 | 外加电位 applied potential |
35 | 水溶液腐蚀 aqueous corrosion |
36 | 人造海水 artificial seawater |
37 | 大气暴露试验 atmospheric exposure test |
38 | 大气腐蚀 atmospheric corrosion |
39 | 奥氏体不锈钢 austenitic stainless steel |
40 | 辅助电极 auxiliary electrode |
41 | 细菌腐蚀 bacteria corrosion |
42 | 贱金属 base metal |
43 | 双金属腐蚀 bimetallic corrosion |
44 | 甘汞电极 calomel electrode |
45 | 甘汞电极电位 calomel electrode potential |
46 | 碳化 carburizing |
47 | 阴极 cathode |
48 | 阴极保护 cathodic protection |
49 | 阴极极化 cathodic polarization |
50 | 阴极电流密度 cathodic current density |
51 | 阴极电流效率 cathodic current efficiency |
52 | 阴极区电解质 catholyte |
53 | 阳离子 cation |
54 | 碱脆 caustic embrittlement |
55 | 空泡作用 cavitation |
56 | 空泡腐蚀 cavitation corrosion |
57 | 空泡损伤 cavitation damage |
58 | 空泡磨蚀 cavitation erosion |
59 | 电池 cell |
60 | 渗镀,渗碳 cementation |
61 | 化学清洗 chemical cleaning |
62 | 化学转化涂层 chemical conversion coating |
63 | 化学钝化 chemical passivation |
64 | 化学镀 chemical(electroless)plating |
65 | 铬酸盐处理(铬化) chromating |
66 | 清洗液 cleaning solution |
67 | 浓差电池 concentration cell |
68 | 接触腐蚀 contact corrosion |
69 | 转换涂层 conversion coating |
70 | 恒变形 constant deflection |
71 | 恒载荷 constant load |
72 | 腐蚀 corrosion |
73 | 腐蚀-磨蚀 corrosion-erosion |
74 | 腐蚀疲劳 corrosion fatigue |
75 | 腐蚀电位 corrosion potential |
76 | 腐蚀控制 corrosion control |
77 | 腐蚀电流 corrosion current |
78 | 腐蚀电流密度 corrosion current density |
79 | 腐蚀疲劳开裂 corrosion fatigue cracking |
80 | 腐蚀疲劳极限 corrosion fatigue limit |
81 | 腐蚀产物 corrosion product |
82 | 腐蚀速率 corrosion rate |
83 | 腐蚀科学 corrosion science |
84 | 腐蚀试验 corrosion test |
85 | 腐蚀失重 corrosion weight loss |
86 | 腐蚀增重 corrosion weight gain |
87 | 电偶 couple |
88 | 电偶作用 couple action |
89 | 开裂 cracking |
90 | 龟裂 crazing |
91 | 缝隙腐蚀 crevice corrosion |
92 | 临界阳极电流密度 critical anodic current density |
93 | 临界浓度 critical concentration |
94 | 临界湿度 critical humidity |
95 | 晶体 crystal |
96 | 辅助电极 counter electrode |
97 | 电流密度 current density |
98 | 去活化作用 deactivation |
99 | 脱合金元素作用 dealloying |
100 | 脱铝 dealuminization |
101 | 去气 deaeration |
102 | 缺陷 defect |
103 | 脱脂 degreasing |
104 | 去矿化物质 demineralization |
105 | 去极化 depolarization |
106 | 腐蚀深度 depth of corrosion |
107 | 沉积物腐蚀 deposit corrosion |
108 | 脱锌 dezincification |
109 | 扩散 diffusion |
110 | 扩散电位 diffusion potential |
111 | 差异充气电池 differential aeration cell |
112 | 极限扩散电流密度diffusion limited current density |
113 | 电流 electric current |
114 | 电位 electric potential |
115 | 电化学电池 electrochemical cell |
116 | 电化学腐蚀 electrochemical corrosion |
117 | 电化学当量 electrochemical equivalent |
118 | 电极 electrode |
119 | 电极电位 electrode potential |
120 | 电极反应 electrode reaction |
121 | 电解质 electrolyte |
122 | 电解 electrolysis |
123 | 电解清洗 electrolytic cleaning |
124 | 电动序 electromotive force(Emf)series |
125 | 负电性电位 electropositive potential |
126 | 电泳沉积 electrophoretic deposition |
127 | 电镀 electroplating |
128 | 正电性电位 electropositive potential |
129 | 静电喷涂层 electrostatic coating |
130 | 脆化 embrittlement |
131 | 磨耗 erosion |
132 | 磨耗腐蚀(或冲击腐蚀) erosion-corrosion |
133 | 平衡电位 equilibrium potential |
134 | 腐蚀极化图 Evans diagram |
135 | 剥蚀 exfoliation corrosion |
136 | 交换电流密度 exchange current density |
137 | 暴露实验 exposure test |
138 | 疲劳 fatigue |
139 | 铁素体 ferrite |
140 | 铁素体不锈钢 ferrite stainless steel |
141 | 丝状腐蚀 filiform corrosion |
142 | 弗拉德电位 Flade potential |
143 | 剥层腐蚀 foliation |
144 | 膜 film |
145 | 微动腐蚀 fretting corrosion |
146 | 燃灰腐蚀 fuel ash corrosion |
147 | 电偶作用 galvanic action |
148 | 伽法尼电池 galvanic cell |
149 | 电偶腐蚀 galvanic corrosion |
150 | 电偶对 galvanic couple |
151 | 电偶序 galvanic series |
152 | 热镀锌 galvanizing |
153 | 恒电流的 galvanoststatic |
154 | 普遍(全面)腐蚀 general corrosion |
155 | 晶界裂纹 grain boundary crack |
156 | 晶粒 grain |
157 | 石墨化腐蚀 graphitic corrosion |
158 | 重量法 gravimetric methods |
159 | 绿锈 green rot |
160 | 哈氏合金 hastelloy |
161 | 热影响区 heat affected zone(HAZ) |
162 | 耐热钢 heat resistant steel |
163 | 热处理 heat treatment |
164 | 高温腐蚀 high temperature corrosion |
165 | 热腐蚀 hot corrosion |
166 | 热镀铝 hot-dip alumizing |
167 | 湿度 humidity |
168 | 氢腐蚀 hydrogen attack |
169 | 氢鼓泡 hydrogen blistering |
170 | 氢损伤 hydrogen damage |
171 | 氢电极 hydrogen electrode |
172 | 氢脆 hydrogen embrittlement |
173 | 氢致开裂 hydrogen induced cracking |
174 | 氢超电压 hydrogen overvoltage |
175 | 氢标 hydrogen scale |
176 | 浸泡实验 immersion test |
177 | 冲蚀 impingement corrosion |
178 | 因科乃尔 Inconel |
179 | 因科罗 Incoloy |
180 | 工业大气 industrial atmosphere |
181 | 缓蚀剂 inhibitor |
182 | 晶间裂纹 intergranular crack |
183 | 不溶性阳极 insoluble anode |
184 | 晶间腐蚀 intergranular corrosion |
185 | 延晶应力腐蚀断裂 intergranular stress corrosion cracking |
186 | 内氧化 interal oxidation |
187 | 内应力 interal stress |
188 | 例子浓差电池 ion concentration cell |
189 | 离子 ion |
190 | 离子注入 ion implantation |
191 | 刀线腐蚀 knife-line corrosion |
192 | 激光釉化 laser glazing |
193 | 层状腐蚀 layer corrosion |
194 | 晶格缺陷 lattic defect |
195 | 液态金属腐蚀 liquid metal corrosion |
196 | 局部作用 local action |
197 | 局部电池 local cell |
198 | 局部腐蚀 local corrosion |
199 | 海洋腐蚀 marine corrosion |
200 | 马氏体 martensite |
201 | 马氏体不锈钢 martensitic stainless steel |
202 | 力学性能 mechanical property |
203 | 金属离子浓差电池 metal ion concentration cell |
204 | 金属喷镀 metal spray |
205 | 金属镀层 metallic coating |
206 | 微生物腐蚀 microbiological corrosion |
207 | 金属粉化 metal dusting |
208 | 混合电位 mixed potential |
209 | 轧制铁鳞 mill scale |
210 | 贵金属 noble metal |
211 | 海军黄铜 navy brass |
212 | 贵电位 noble potential |
213 | 非金属涂层 nonmetallic coating |
214 | 氮化 nitriding |
215 | 过电位 overpotential |
216 | 氧化 oxidation |
217 | 开路电位 open circuit potential |
218 | 氧化-还原电位 oxidation-reduction potential |
219 | 氧化物 oxide |
220 | 氧化膜 oxide film |
221 | 氧浓差电池 oxygen concentration cell |
222 | 钝化 passivation |
223 | 钝化剂 passivator |
224 | 钝化-活化电池 passive-active cell |
225 | 钝化的,钝性的 passive |
226 | 铜绿 patina |
227 | 酸度计 pH indicator,acidometer |
228 | 磷酸盐处理 phosphating |
229 | 酸洗液 pickling solution |
230 | 蚀孔 pit |
231 | 点蚀 pitting |
232 | 点蚀击穿电位 pitting breakdown potential |
233 | 点蚀系数 pitting factor |
234 | 点蚀电位 pitting potential |
235 | 极化 polarization |
236 | 动电位 potential dynamic(potentiokinetic) |
237 | 恒电位仪 potentiostat |
238 | 恒电位 potentisostic |
239 | 电位-pH图 Pourbaix diagram,potential-pH diagram |
240 | 底涂层 prime coat |
241 | 保护电位 protective potential |
242 | 氧化-还原电位 redox potential |
243 | 还原 reduction |
244 | 参比电极 reference electrode |
245 | 相对湿度 relative humidity |
246 | 残余内应力 residua interal stress |
247 | 铁锈 rust |
248 | 防锈油 rust preventive oil |
249 | 牺牲阳极保护 sacrifice anode protection |
250 | 盐水喷雾试验 salt spray test |
251 | 喷砂 sand blasting |
252 | 饱和甘汞电极 saturated calomel electrode(SCE) |
253 | 氧化皮 scale |
254 | 季裂 season cracking |
255 | 选择性腐蚀 selective corrosion |
256 | 选择性氧化 selective oxidation |
257 | 自钝化 self passivation |
258 | 敏化热处理 sensitizing heat treatment |
259 | 喷丸 shot peening |
260 | 银-氯化银电极 silver-sliver chloride electrode |
261 | 慢应变速率 slow strain rate |
262 | 土壤腐蚀 soil corrosion |
263 | 剥离 spalling |
264 | 不锈钢 stainless steel |
265 | 标准电极电位 standard electrode potential |
266 | 标准氢电极 standard hydrogen electrode |
267 | 应变能 strain energy |
268 | 杂散电流腐蚀 stray current corrosion |
269 | 应力场强度因子 stress intensity factor |
270 | 应力腐蚀断裂 stress corrosion cracking(SCC) |
271 | 硫化 sulfidation |
272 | 表面氧化 surface oxidation |
273 | 表面处理 surface treatment |
274 | 皮下腐蚀 subsurface corrosion |
275 | 塔菲尔斜率 Tafel slope |
276 | 失泽 tarnish |
277 | 抗拉强度 tensile strength |
278 | 热偶腐蚀 thermogalvanic corrosion |
279 | 热力学 thermodynamics |
280 | 结瘤腐蚀 tuberculation |
281 | 穿晶腐蚀 transgranular corrosion |
282 | 穿晶应力腐蚀断裂 transgranular stress corrosion cracking |
283 | 过钝化 transpassive |
284 | 膜下腐蚀 underfilm corrosion |
285 | 均匀腐蚀 umiform corrosion |
286 | 水线腐蚀 waterline corrosion |
287 | 焊接腐蚀 weld decay |
288 | 湿度 humidity |
289 | 工作电极 working electrode |
更多关于材料方面、材料腐蚀控制、材料科普等方面的国内外最新动态,我们网站会不断更新。希望大家一直关注中国腐蚀与防护网http://www.ecorr.org
责任编辑:王元
《中国腐蚀与防护网电子期刊》征订启事
投稿联系:编辑部
电话:010-62313558-806
邮箱:fsfhzy666@163.com
中国腐蚀与防护网官方 QQ群:140808414
免责声明:本网站所转载的文字、图片与视频资料版权归原创作者所有,如果涉及侵权,请第一时间联系本网删除。
相关文章
无相关信息

官方微信
《中国腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62313558-806
- 邮箱:fsfhzy666@163.com
- 中国腐蚀与防护网官方QQ群:140808414