ISO/TC156-国际标准化组织金属和合金的腐蚀技术委员会,成立于1974年,现秘书处为中国国家标准化管理委员会(SAC),由冶金工业信息标准化研究院承担秘书处工作。
工作范围:金属和合金腐蚀领域的标准化,包括腐蚀试验方法、腐蚀防护方法、腐蚀控制工程生命周期管理。
现在已出版的金属和合金的腐蚀ISO国际标准有:
(1) ISO 3079:2022 Two-electrode method using acetic acid to measure pitting potential of aluminium and aluminium alloys in chloride solutions用醋酸测定氯化物溶液中铝和铝合金点蚀电位的双电极法
(2) ISO 3651-1:1998 Determination of resistance to intergranular corrosion of stainless steel - Part 1: Austenitic and ferritic- austentic(duplex) stainless steels - Corrosion test in nitric acid medium by measurement of loss in mass(Huey test)不锈钢耐晶间腐蚀的测定-方法1:奥氏体、铁素体-奥氏体(双相)在硝酸中的腐蚀试验(失重法-Huey法)
(3) ISO 3651-2:1988 Determination of resistance to intergranular corrosion of stainless steel - Part 2: Ferritic, austenitic and ferritic-austenitic(duplex) stainless steels - Corrosion test in media containing sulfuric acid不锈钢耐晶间腐蚀的测定-方法2:奥氏体、铁素体-奥氏体(双相)在硫酸中的腐蚀试验
(4) ISO 3651-3:2017 Determination of resistance to intergranular corrosion of stainless steel - Part 3: Corrosion test for low-Cr ferritic stainless steels不锈钢耐晶间腐蚀的测定-方法3:低铬铁素体不锈钢腐蚀试验
(5) ISO 4212:2023 Corrosion of metals and alloys - Method of oxalic acid etching test for intergranular corrosion of austenitic stainless steel 金属和合金的腐蚀-奥氏体不锈钢晶间腐蚀-草酸浸蚀试验方法
(6) ISO 4215:2022 Corrosion of metals and alloys - Test method for high-temperature corrosion testing of metallic materials by thermogravimetry under isothermal or cyclic conditions 金属和合金的腐蚀-在等温或循环条件下用热重法测定金属材料高温腐蚀试验方法
(7) ISO 4680:2022 Corrosion of metals and alloys - Uniaxial constant-load test method for evaluating susceptibility of metals and alloys to stress corrosion cracking in high-purity water at high temperatures 金属和合金的腐蚀-评价高温下高纯水中金属和合金应力腐蚀开裂敏感性的单轴恒载荷试验方法
(8) ISO 4905:2023 Corrosion of metals and alloys - Electrochmical test methods for high-temerature corrosion testing of metallic materials in molten salts 金属和合金的腐蚀-熔盐中金属材料高温腐蚀试验的电化学试验方法
(9) ISO 5156:2022 Corrosion of metals and alloys - Corrosion test method for disinfectant - Total immersion method 金属和合金的腐蚀-消毒剂腐蚀试验方法-全浸法
(10) ISO 5668 Corrosion of metals and alloys - Guidelines and requirements for corrosion testing in simulated environment of deep-sea water 金属和合金的腐蚀-深海模拟环境腐蚀腐蚀导则和要求
(11) ISO 6509-1:2014 Corrosion of metals and alloys - Determination of dezincification resistance of copper alloys with zinc - Part 1: Test method 金属和合金的腐蚀-含锌铜合金抗脱锌性能的测试-第1部分:试验方法
(12) ISO 6509-2:2017 Corrosion of metals and alloys - Determination of dezincification resistance of copper alloys with zinc - Part 2: Assessment criteria 金属和合金的腐蚀-含锌铜合金抗脱锌性能的测试-第2部分:评定标准
(13) ISO 7384:1986 Corrosion tests in artificial atmosphere - General requirements 人造大气腐蚀试验-一般要求
(14) ISO 7441:2015 Corrosion of metals and alloys - Determination of bimetallic corrosion in atmospheric exposure corrosion tests大气暴露腐蚀试验中双金属腐蚀的测定
(15) ISO 7539-1:2012 Corrosion of metals and alloys - Stress corrosion testing - Part 1: General guidance on testing procedures 金属和合金的腐蚀-应力腐蚀试验-第1部分:试验方法总则
(16)ISO 7539-2:1989 Corrosion of metals and alloys - Stress corrosion testing - Part 2: Preparation and use of bent-beam specimens 金属和合金的腐蚀-应力腐蚀试验-第2部分:弯梁试样的制备和应用
(17)ISO 7539-3:1989 Corrosion of metals and alloys - Stress corrosion testing - Part 3: Preparation and use of U-bend specimens 金属和合金的腐蚀-应力腐蚀试验-第3部分:U型弯曲试样的制备和应用
(18)ISO 7539-4:1989 Corrosion of metals and alloys - Stress corrosion testing - Part 4: Preparation and use of uniaxially loaded tension specimens 金属和合金的腐蚀-应力腐蚀试验-第4部分:单轴加载拉伸试样的制备和应用
(19)ISO 7539-5:1989 Corrosion of metals and alloys - Stress corrosion testing - Part 5: Preparation and use of C -ring specimens 金属和合金的腐蚀-应力腐蚀试验-第5部分:C 型环试样的制备和应用
(20)ISO 7539-6:1989 Corrosion of metals and alloys - Stress corrosion testing - Part 6: Preparation and use of precracked specimens for tests under constant load or constant displacement 金属和合金的腐蚀-应力腐蚀试验-第6部分:恒载荷或恒位移条件下预制裂纹试样的制备和应用
(21)ISO 7539-7:2005 Corrosion of metals and alloys - Stress corrosion testing - Part 7: Method for slow strain rate testing 金属和合金的腐蚀-应力腐蚀试验-第7部分:慢应变速率试验
(22)ISO 7539-8:2000 Corrosion of metals and alloys - Stress corrosion testing - Part 8: Preparation and used of specimens to evaluate weldments 金属和合金的腐蚀-应力腐蚀试验-第8部分:焊接试样的制备和应用
(23)ISO 7539-9:2021 Corrosion of metals and alloys - Stress corrosion testing - Part 9: Preparation and used of pre-cracked specimens for tests under rising load or rising displacement 金属和合金的腐蚀-应力腐蚀试验-第9部分:渐增式载荷或渐增式位移条件下的预制裂纹试样的制备和应用
(24)ISO 7539-10:2020 Corrosion of metals and alloys - Stress corrosion testing - Part 10: Reverse U-bend method金属和合金的腐蚀-应力腐蚀试验-第10部分:反向U型弯曲试验方法
(25)ISO 7539-11:2013 Corrosion of metals and alloys - Stress corrosion testing - Part 11:Guidelines for testing the resistance of metals and alloys to hydrogen embrittlement and hydrogen-assisted cracking 金属和合金的腐蚀-应力腐蚀试验-第11部分:金属和合金氢脆和氢致开裂试验指南
(26)ISO/FDIS 7539-12 Corrosion of metals and alloys - Stress corrosion testing - Part 12: Requirements for atmospheric stress corrosion cracking testing 金属和合金的腐蚀-应力腐蚀试验-第12部分:大气应力腐蚀开裂试验要求(待发布)
(27)ISO/TR 7655:2022 Corrosion of metals and alloys - Overview of metal corrosion protection when using disinfectants 金属和合金的腐蚀-使用消毒剂时金属腐蚀防护概述
(28)ISO 8044:2020 Corrosion of metals and alloys - Vocabulary 金属和合金的腐蚀-术语
(29)ISO 8407:2021 Corrosion of metals and alloys - Removal of corrosion products from corrosion test specimens 金属和合金的腐蚀 腐蚀试样上腐蚀产物的清除
(30)ISO 8565:2011 Metals and alloys - Atmospheric corrosion testing - GEneral requirements 金属和合金-大气腐蚀试验-一般要求