1 金属材料疲劳、断裂试验标准
(1) ASTM 相关标准
ASTM E739 线性或线性化应力-寿命(S-N)和应变-寿命(e-N)
ASTM E647 疲劳裂纹扩展速率试验方法
ASTM E468 Standard Practice for Presentation of Constant Amplitude Fatigue Test Results for Metallic Materials
ASTM E466 金属材料力控制恒幅轴向疲劳试验方法
ASTM E399 Standard Test Method for Linear-Elastic Plane-Strain Fracture Toughness of Metallic Material
ASTM E561 Standard Test Method for K-R Curve Determination
ASTM E740 Standard Practice for Fracture Testing with Surface-Crack Tension Specimens
ASTM E1152 Standard Test Method for determining J-R Curves
ASTM E1820 Standard Test Method for Measurement of Fracture Toughness
ASTM E606/E606M Standard Test Method for Strain-Controlled Fatigue Testing
ASTM E1942 Standard Guide for Evaluating Data Acquisition Systems Used in Cyclic Fatigue and Fracture Mechanics Testing
ASTM E2472 Standard Test Method for Determination of Resistance to Stable Crack Extension under Low-Constraint Conditions
ASTM B646 Standard Practice for Fracture Toughness Testing of luminum Alloys
ASTM E2818 Standard Practice for Determination of Quasistatic Fracture Toughness of Welds
(2) GB相关标准
GB/T 3075 金属轴向疲劳试验方法
GB/T 6398 金属材料裂纹扩展试验方法
GB/T 4337 金属旋转弯曲疲劳试验方法
GB/T 7733 金属旋转弯曲腐蚀疲劳试验方法
GB/T 12443 金属扭应力疲劳试验方法
GB/T 7732 金属材料表面裂纹拉伸试样断裂韧度试验方法
GB/T 21143 金属材料准静态断裂韧度的统一试验方法
GB/T 24176 金属材料疲劳试验数据统计方案与分析方法
GB/T 2107 金属高温旋转弯曲疲劳试验方法
GB/T15248 金属材料轴向等幅低循环疲劳试验方法
GB/T10622 金属材料滚动接触疲劳试验方
GB/T 4161 金属材料平面应变断裂韧度试验方法
GB/T 2038 金属材料延性断裂韧度试验方法
GB/T 26077 金属材料疲劳试验轴向应变控制方法
GB/T 26076 金属薄板(带)轴向力控制疲劳试验方法
GB/T 27595 胶粘剂结构胶粘剂拉伸剪切疲劳性能的试验方法
GB/T 12443 金属材料扭应力疲劳试验方法
GB/T 13682 螺纹紧固件轴向疲劳试验方法
GB/T 30064 金属材料钢构件断裂评估中裂纹尖端张开位移(CTOD)断裂韧度的拘束损失修正方法
GB/T 24522 金属材料低拘束试样测定稳定裂纹扩展阻力的试验方法
GB/T 28896 金属材料焊接接头准静态断裂韧度测定的试验方法
GB/T 27551 金属材料焊缝破坏性试验断裂试验
(3) HB相关标准
HB 5142 金属材料平面应变断裂韧度试验方法
HB 5152 金属室温旋转弯曲疲劳试验方法
HB 5153 金属高温旋转弯曲疲劳试验方法
HB 5217 金属低周热疲劳试验方法
HB 5277 发动机叶平及材料振动疲劳试验方法
HB 5287 金属材料轴向加载疲劳试验方法
HB 5279 金属板材表面裂纹断裂韧性试验方法
HB 5487 铝合金断裂韧度试验方法
HB 6626 金属材料在含水介质中疲劳裂纹扩展速率试验方法
HB 7572 金属材料(人字形缺口)平面应变断裂韧度试验方法
HB 7680 金属材料高温疲劳裂纹扩展速率试验方法
HB 7705 金属材料疲劳小裂纹扩展速率试验方法
HB 6442 飞机液压导管及连接件弯曲疲劳试验
HB 7680 高温疲劳裂纹扩展速率试验方法
HB 5261 金属板材K-R曲线试验方法
HB 6660 金属板材热疲劳试验方法
HB 7110 金属材料细节疲劳额定强度截止值(DFRcutoff)试验方法
HB/Z 112 材料疲劳试验统计分析方法
HB 20041 航空发动机轴类部件疲劳试验方法
(4) GJB相关标准
GJB 2030 高温下金属材料断裂韧度试验方法
GJB 1997 金属材料轴向腐蚀疲劳试验方法
GJB 715.30A 紧固件试验方法-拉伸疲劳
GJB 715.30 紧固件试验方法-抗拉疲劳
GJB 715.9 紧固件试验方法-抗剪接头疲劳
2 复合材料疲劳、断裂试验标准
(1) ASTM相关标准
ASTM D5528 Standard Test Method for ModeI Interlaminar Fracture Toughness of Unidirectional Fiber-Reinforced Polymer Matrix Composites
ASTM D3479/D3479 MStandard Test Method for Tension-Tension Fatigue of Polymer Matrix Composite Materials
ASTM D7774 Standard Test Method for Flexural Fatigue Properties of Plastics
ASTM D7791 Standard Test Method for Uniaxial Fatigue Properties of Plastics
ASTM D4482 Standard Test Method for Rubber Property-ExtensionCycling Fatigue
ASTM D7615/D7615M Standard Practice for Open-Hole Fatigue Response of Polymer Matrix Composite Laminates
ASTM D3166 Standard Test Method for Fatigue Properties of Adhesives in Shear by Tension Loading (Metal/Metal)
ASTM D6115 Standard Test Method for ModeI Fatigue Delamination Growth Onset of Unidirectional Fiber-Reinforced Polymer atrixComposites
ASTM E1049 Standard Practices for Cycle Counting in Fatigue Analysis
(2) GB相关标准
GB/T 16779 纤维增强塑料层合板拉-拉疲劳性能试验方法
GB/T 28891-2012 纤维增强塑料复合材料单向增强材料Ⅰ型层间断裂韧性的测定
(3) HB相关标准
HB 7624 碳纤维复合材料层合板弯曲疲劳试验方法
HB 5268 有机玻璃板材断裂韧度试验方法
HB 7402 碳纤维复合材料层合板I型层间断裂韧性试验方法
HB 7403 碳纤维复合材料层合板II型层间断裂韧性试验方法
HB 7718.1 碳纤维复合材料层合板湿热环境下层间断裂韧性试验方法第1部分:I型层间断裂韧性试验方法
HB 7718.2 碳纤维复合材料层合板湿热环境下层间断裂韧性试验方法第2部分:II型层间断裂韧性试验方法
(4) GJB相关标准
GJB 586 纤维增强塑料层板拉伸层间断裂韧性试验方法
GJB 2637 碳纤维树脂基复合材料层合板疲劳试验方法
GJB 2033 航空有机玻璃拉伸疲劳试验方法
免责声明:本网站所转载的文字、图片与视频资料版权归原创作者所有,如果涉及侵权,请第一时间联系本网删除。
官方微信
《中国腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62316606-806
- 邮箱:fsfhzy666@163.com
- 中国腐蚀与防护网官方QQ群:140808414