精美Al-Si合金金相图片
![1.jpg](/d/file/news/industry/2018-12-26/f7e38c3dfec31fda5945e147aed4278e.jpg)
![1.2.jpg](/d/file/news/industry/2018-12-26/bd538b307ab2771af7e34e58a4533c43.jpg)
01 99.999%Al, 已变形的晶粒结构
![2.jpg](/d/file/news/industry/2018-12-26/e878d6a603d14bfaab821ff18a480ad5.jpg)
![2.2.jpg](/d/file/news/industry/2018-12-26/80b6609f558b9325897f50a627609a43.jpg)
02 Al-1%Si 铸造合金样品,在初生α铝基体中可见硅粒子。
![3.jpg](/d/file/news/industry/2018-12-26/822905faa2dad902a99872d53b5ac75f.jpg)
![3.3.jpg](/d/file/news/industry/2018-12-26/9474edfde580d390cd9ff21561224529.jpg)
03 Al-7%Si, 铸态组织,初生α枝晶和α-Al/Si共晶
![4.jpg](/d/file/news/industry/2018-12-26/301c18e19b1caaac19b20246f6649038.jpg)
![4.4.jpg](/d/file/news/industry/2018-12-26/be05ce773a59d836ce94b877b7d910bc.jpg)
04 Al-11%Si, 铸态组织,初生α枝晶和α-Al/Si共晶
![5.jpg](/d/file/news/industry/2018-12-26/03d2a7a33cce292c194b09485b08b055.jpg)
![.5.jpg](/d/file/news/industry/2018-12-26/637b98d3de1a9cd70c2287a9faea6522.jpg)
05 Al-12%Si, 铸态组织,近共晶
![6.jpg](/d/file/news/industry/2018-12-26/ba5fee576e1be16ad030f54d1de06a35.jpg)
![6.6.jpg](/d/file/news/industry/2018-12-26/29814a86b682248ca792bd2cefea2727.jpg)
06 Al-12%Si, 铸态组织,近共晶
![7.jpg](/d/file/news/industry/2018-12-26/3c51862fd87cd6830439480c77f01b96.jpg)
![13.1.jpg](/d/file/news/industry/2018-12-26/c3377e11257c452c7b3488224a4d9ded.jpg)
07 Na改性Al-12%Si, 铸态组织,近共晶
![8.jpg](/d/file/news/industry/2018-12-26/24790e0bb9ec59cd0a32905f73e266fe.jpg)
![8.8.jpg](/d/file/news/industry/2018-12-26/f009d09f5468cf8aa546b644d194a9d1.jpg)
08 Na改性Al-12%Si, 铸态组织,近共晶
![9.jpg](/d/file/news/industry/2018-12-26/a87dfe135b25c501d2be84cbe4b0a833.jpg)
![9.9.jpg](/d/file/news/industry/2018-12-26/62fff5f335f49e49f3a10e21b39bf882.jpg)
09 Al-12.9%Si, 重力铸造
![10.jpg](/d/file/news/industry/2018-12-26/22301ca97e39caa5adc225d3db47edae.jpg)
![10.1.jpg](/d/file/news/industry/2018-12-26/7f368d2f7152ebd45f202a114efbe98a.jpg)
10 Al-12%Si-0.04%Sr, 重力铸造
![11.jpg](/d/file/news/industry/2018-12-26/3ebd66afca8de8bd0eade173d9f2ae60.jpg)
![11.1.jpg](/d/file/news/industry/2018-12-26/2fa1da4a4fe4c477232e2db5c4d55d8e.jpg)
11 Al-19.85%Si,铸造,过共晶,初生Si加共晶
12 Al-25%Si,铸造,过共晶,初生Si加α-Al/Si共晶
13 Al-50%Si,铸造,过共晶,初生Si开裂加共晶
14 99.9999%Si,铸造,75%NaOH溶液
15 Al-Si相图
更多关于材料方面、材料腐蚀控制、材料科普等方面的国内外最新动态,我们网站会不断更新。希望大家一直关注中国腐蚀与防护网http://www.ecorr.org
责任编辑:王元
《中国腐蚀与防护网电子期刊》征订启事
投稿联系:编辑部
电话:010-62313558-806
邮箱:fsfhzy666@163.com
中国腐蚀与防护网官方 QQ群:140808414
免责声明:本网站所转载的文字、图片与视频资料版权归原创作者所有,如果涉及侵权,请第一时间联系本网删除。
相关文章
![](/skin/201904/index/img/ssdf.png)
官方微信
《中国腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62313558-806
- 邮箱:fsfhzy666@163.com
- 中国腐蚀与防护网官方QQ群:140808414
点击排行
PPT新闻
“海洋金属”——钛合金在舰船的
点击数:5768
腐蚀与“海上丝绸之路”
点击数:4763