盐雾试验是一种主要利用盐雾试验设备所创造的人工模拟盐雾环境条件来考核产品或金属材料耐腐蚀性能的环境试验,它与天然环境相比,其盐雾环境的氯化物的盐浓度,可以是一般天然环境盐雾含量的几倍或几十倍,使腐蚀速度大大提高,对产品进行盐雾试验,得出结果的时间也大大缩短。盐盐雾试验方法有:中性盐雾(NSS)试验、醋酸盐雾(ASS)试验、铜加速的醋酸盐雾(CASS)试验等。
总体概况
盐雾试验是一种主要利用盐雾试验设备所创造的人工模拟盐雾环境条件来考核产品或金属材料耐腐蚀性能的环境试验,它与天然环境相比,其盐雾环境的氯化物的盐浓度,可以是一般天然环境盐雾含量的几倍或几十倍,使腐蚀速度大大提高,对产品进行盐雾试验,得出结果的时间也大大缩短。盐盐雾试验方法有:中性盐雾(NSS)试验、醋酸盐雾(ASS)试验、铜加速的醋酸盐雾(CASS)试验等。
盐雾试验相关技术标准
标准名称:耐中性盐雾性能的测试
标准编号:GB/T 1771-1991
发布日期:1991-08-24
实施日期:1992-08-01
标准概述:本标准规定了测定涂层耐中性盐雾性能的方法。本标准所规定的方法可以作为色漆或涂料体系质量的检测手段。
标准名称:人造气氛腐蚀试验 盐雾试验
标准编号:GB/T10125-1997
发布日期:1997-06-27
实施日期:1998-01-01
标准概述:本标准考虑到试验初期试样的变化较大,并为满足国内各类产品的需要,将推荐的试验周期定为2 h,4 h,6 h,8 h,24 h,48 h,96 h,168 h,240 h,480 h,720 h,l 000 h;与ISO 9227:1990比较,增加了4h和8 h.
标准名称:Standard Practice for Operating Salt Spray (Fog) Apparatus
标准编号:B117 ? 11
标准概述:This standard is issued under the ?xed designation B117; the number immediately following the designation indicates the year of original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval. A superscript epsilon (ε) indicates an editorial change since the last revision or reapproval.This standard has been approved for use by agencies of the Department of Defense.
标准名称:Standard Test Method for Copper-Accelerated Acetic Acid-Salt Spray (Fog) Testing(CASS Test)
标准编号:B368 ? 09
标准概述:This standard is issued under the ?xed designation B368; the number immediately following the designation indicates the year of original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval. A superscript epsilon (ε) indicates an editorial change since the last revision or reapproval.This standard has been approved for use by agencies of the Department of Defense.
标准名称:Standard Practice for Determining Cracking Susceptibility of Metals Exposed Under Stress to a Hot Salt Environment
标准编号:ASTM G41?90
标准概述:This standard is issued under the ?xed designation G41; the number immediately following the designation indicates the year of original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval. A superscript epsilon (ε) indicates an editorial change since the last revision or reapproval.
标准名称:Standard Practice for Modi?ed Salt Spray (Fog) Testing
标准编号:ASTM G85?11
标准概述:This standard is issued under the ?xed designation G85; the number immediately following the designation indicates the year of original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval. A superscript epsilon (ε) indicates an editorial change since the last revision or reapproval.This standard has been approved for use by agencies of the Department of Defense.
标准名称:Corrosion tests in artificial atmospheres-Salt spray tests
标准编号:ISO 9227:2012
标准概述:Salt spray tests are generally suitable as corrosion protection tests for rapid analysis for discontinuties, pores and damage in organic and inorganic coatings.In addition, for quality control purpose, comparison can be made between specimens coated with the same coating. As comparative tests; however, salt spray tests are only suitable if the coatings are sufficiently similar in nature.It is often not possible to use results gained from salt spray testing as a comparative guide to the long-term behaviour of different coating systems, since the corrosion stress during these tests differs significantly from the corrosion stresses encountered in practice.