将金属基材和水性介质物理隔绝的超疏水涂层成为一种有前景金属防腐蚀策略,但其实际应用受限于在严苛环境中的机械耐久性差和性能快速退化。
本文要点
这项工作提出了一种仿生策略用于开发兼具超疏水性、自修复和实时损伤感知的智能防腐蚀涂层,推进了MOF衍生材料在防护涂层中的应用。
Chengliang Zhou (周城良) received his Bachelor’s degree in applied chemistry from Hunan Agricultural University. He received a PhD degree in chemical engineering and technology from Hunan University. His research focuses on bioinspired design and fabrication of self-healing nanocomposites and biobased polymer materials, with applications in functional coatings and smart corrosion control.
Xiaohu Luo (罗小虎) is currently an associate professor at the School of Chemistry and Chemical Engineering, Qiannan Normal University for Nationalities, and is the director of the Engineering Research Center of Lose Efficacy and Anticorrosion of Materials of Guizhou. His research focuses on green and highly efficient corrosion inhibitors and multifunctional coatings.
Yali Liu (刘娅莉) is a professor at the College of Chemistry and Chemical Engineering, Hunan University. She is the deputy director of the Technical Committee on Coating and Surface Protection Technology, Chinese Society for Corrosion and Protection. Her research focuses on metal corrosion and protection, functional and smart coatings, surface treatment, and biobased polymer materials.
Xingong Li (李新功) is currently a professor at the College of Materials and Energy, Central South University of Forestry and Technology. He has received the honorary title of “Young and Middle-aged Experts with Outstanding Contributions” and has been selected in the National Millions of Talents Project in the New Century and the Hunan Provincial “121” Talent Project. His research focuses on interfacial design and fabrication of green and multifunctional composite materials.
Hongbo Zeng (曾宏波) is a professor at the Department of Chemical and Materials Engineering, the University of Alberta and a Tier 1 Canada Research Chair in intermolecular forces and interfacial science, and he is recognized as a Fellow of the Royal Society of Canada’s Academy of Science, the Canadian Academy of Engineering, and the Royal Society of Chemistry. He received his BSc and MSc degrees at Tsinghua University, followed by a PhD degree at the University of California, Santa Barbara. Zeng’s research interests are mainly in colloid and interface science, functional materials & nanotechnology, with a specific focus on the intermolecular and surface interactions in soft materials (e.g., polymers, biopolymers) and engineering processes.
文章信息 https://doi.org/10.1007/s40843-025-3572-6
免责声明:本网站所转载的文字、图片与视频资料版权归原创作者所有,如果涉及侵权,请第一时间联系本网删除。
官方微信
《腐蚀与防护网电子期刊》征订启事
- 投稿联系:编辑部
- 电话:010-62316606
- 邮箱:fsfhzy666@163.com
- 腐蚀与防护网官方QQ群:140808414